Optimization of the treatment process of zinc leaching residue by using the response surface method

Abstract: The decrease in the zinc volatilization rate is usually due to the liquid phase, which is typically generated in the rotary kiln. The response surface model was built to analyze and explore the effects of carbon content, basicity, and holding time on the zinc volatilization rate and residue state. Moreover, the model was used to optimize the experimental conditions. The results showed that the effect of basicity on zinc volatilization rate was statistically significant, whereas the effects of carbon content and holding time were relatively small. The optimized process conditions were as follows: carbon content of 32%, basicity of 3, and holding time of 30 min. Under this condition, the zinc volatilization rate was 99.65%, and the furnace residue was sintered, which proved to be beneficial to the subsequent step of iron extraction.

Standort
Deutsche Nationalbibliothek Frankfurt am Main
Umfang
Online-Ressource
Sprache
Englisch

Erschienen in
Optimization of the treatment process of zinc leaching residue by using the response surface method ; volume:7 ; number:5 ; year:2018 ; pages:460-463 ; extent:4
Green processing & synthesis ; 7, Heft 5 (2018), 460-463 (gesamt 4)

Urheber
Ma, Hongzhou
Xie, Hongwei
Wang, Yaoning
Yan, Chao

DOI
10.1515/gps-2017-0043
URN
urn:nbn:de:101:1-2501120412334.100511002852
Rechteinformation
Open Access; Der Zugriff auf das Objekt ist unbeschränkt möglich.
Letzte Aktualisierung
15.08.2025, 07:23 MESZ

Datenpartner

Dieses Objekt wird bereitgestellt von:
Deutsche Nationalbibliothek. Bei Fragen zum Objekt wenden Sie sich bitte an den Datenpartner.

Beteiligte

  • Ma, Hongzhou
  • Xie, Hongwei
  • Wang, Yaoning
  • Yan, Chao

Ähnliche Objekte (12)