Oxidation Behavior of Ferritic Steel T22 Exposed to Supercritical Water

Abstract: The oxidation tests of Ferritic Steel T22 exposed to supercritical water (SCW) at 540–620°C and 25 MPa was performed for up to 1000 h. The oxidation rate increased with increasing exposure temperature and time. Oxide films formed on T22 have a double-layered structure with an outer layer consisting of iron oxide and an inner layer consisting of spinel oxide. Numerous pores on the surface can be observed at the initial oxidation stage while they seemed to heal with increasing exposure time at 620°C. Cracks occurred along grain boundaries in the oxide scale when T22 exposed for 200 h at 620°C. The influence of time and temperature on the oxidation of Ferritic Steel T22 was discussed.

Location
Deutsche Nationalbibliothek Frankfurt am Main
Extent
Online-Ressource
Language
Englisch

Bibliographic citation
Oxidation Behavior of Ferritic Steel T22 Exposed to Supercritical Water ; volume:38 ; number:2019 ; year:2019 ; pages:476-484 ; extent:9
High temperature materials and processes ; 38, Heft 2019 (2019), 476-484 (gesamt 9)

Creator
Zhu, Zhongliang
Khan, Hasan Izhar
Cao, Qi
Zhang, Naiqiang

DOI
10.1515/htmp-2018-0100
URN
urn:nbn:de:101:1-2501280351521.503424890363
Rights
Open Access; Der Zugriff auf das Objekt ist unbeschränkt möglich.
Last update
15.08.2025, 7:38 AM CEST

Data provider

This object is provided by:
Deutsche Nationalbibliothek. If you have any questions about the object, please contact the data provider.

Associated

  • Zhu, Zhongliang
  • Khan, Hasan Izhar
  • Cao, Qi
  • Zhang, Naiqiang

Other Objects (12)