High-Temperature Graphitization Failure of Primary Superheater Tube

Abstract: Failure of boiler tubes is the main cause of unit outages of the plant, which further affects the reliability, availability and safety of the unit. So failure analysis of boiler tubes is absolutely essential to predict the root cause of the failure and the steps are taken for future remedial action to prevent the failure in near future. This paper investigates the probable cause/causes of failure of the primary superheater tube in a thermal power plant boiler. Visual inspection, dimensional measurement, chemical analysis, metallographic examination and hardness measurement are conducted as the part of the investigative studies. Apart from these tests, mechanical testing and fractographic analysis are also conducted as supplements. Finally, it is concluded that the superheater tube is failed due to graphitization for prolonged exposure of the tube at higher temperature.

Location
Deutsche Nationalbibliothek Frankfurt am Main
Extent
Online-Ressource
Language
Englisch

Bibliographic citation
High-Temperature Graphitization Failure of Primary Superheater Tube ; volume:34 ; number:8 ; year:2015 ; pages:777-781 ; extent:5
High temperature materials and processes ; 34, Heft 8 (2015), 777-781 (gesamt 5)

Creator
Ghosh, D.
Ray, S.
Roy, H.
Mandal, N.
Shukla, A. K.

DOI
10.1515/htmp-2014-0137
URN
urn:nbn:de:101:1-2501270536592.479372569765
Rights
Open Access; Der Zugriff auf das Objekt ist unbeschränkt möglich.
Last update
15.08.2025, 7:24 AM CEST

Data provider

This object is provided by:
Deutsche Nationalbibliothek. If you have any questions about the object, please contact the data provider.

Associated

  • Ghosh, D.
  • Ray, S.
  • Roy, H.
  • Mandal, N.
  • Shukla, A. K.

Other Objects (12)